Care of Epoxy Floors

November 1, 2016

Epoxy Flooring Systems and Coatings

Daily Maintenance of Seamless Flooring and Floor Coatings

  • Sweep the floors daily.epoxy_chip_flooring_263s
  • If abrasive particles  are present they should be removed by mopping with common household detergents and rinsed completely.  Be sure not to use the detergent at a concentration higher than that recommended by the manufacturer of the floor cleaning material.  Be sure to test any cleaner that you haven’t used before on a sample of the Seamless Flooring Material or Seamless Floor coating.  You may want to be sure to prepare these samples as you are installing the floor so they will be available to you at a later time.
  • Promptly remove grease, and other contaminants from the surface of the floor
  • Be sure to rinse off all chemical solutions that may attack the surface.

Weekly Maintenance of Seamless Flooring and Floor Coatings

Smooth Systems

All seamless flooring and floor coatings should be mopped on a regular bases with a neutral soap or detergent, and completely rinsed. Be sure not to use the detergent at a concentration higher than that recommended by the manufacturer of the floor cleaning material.

Be sure to test any cleaner that you haven’t used before on a sample of the Seamless Flooring Material or Seamless Floor coating.

Mop should be rinsed often. Synthetic mops tend to work better on textured surfaces than cotton mops. The water should be changed frequently as well. Smooth floors are easily cleaned this way. It may be necessary to give extra care to areas that are subject to heavy traffic, hard rubber wheels, and steel wheels that leave marks. In these situations you can use the methods used for textured floors for these more difficult to remove contamination.

Textured Systems

Textured systems may require the use of a stiff bristled brush or floor scrubber to reach to bottom of the anti-skid texture.  Severe problem areas can be treated as follows:

Grease Removal

Grease is typically removed by Tri-sodium phosphate (TSP) or other commonly available biodegradable cleaner. Contact Epoxy.comTechnical Support Department with your specific questions.

Removing Dairy Products

Dairy products should be removed immediately as they may cause staining on some types of seamless flooring and seamless floor coating systems.

Tire Marks Removal

Scrub the area(s) with a stiff bristled brush and using the same biodegradable floor cleaner that you are using to mop with.

Stubborn Dirt or Stain Removal

When you are trying to remove stubborn dirt or stains,allow the biodegradable cleaner to set in the area for a little while longer and do the work for you. Then completely rinse to area to remove the cleaner and the dirt.

Chemical Spills

You should always rinse strong chemicals as quickly as possible completely from the surface. Chemicals allowed to dry on the surface typically become more concentrated as they dry.  That may cause the chemical to get concentrated enough to stain or even attack the seamless floor or seamless floor coating.

Waxing and Polishing of Seamless Flooring and Seamless Floor Coatings

Epoxy.com Epoxy and Urethane Seamless Flooring and Seamless Floor Coating Systems are very shinny and so waxing or polishing are not necessary.  If a floor is very old, or has seen extremely high traffic this shine may dull.  If it does then you can wax or polish the floor with standard commercial products that are designed for that purpose. Better yet, if this happens, you may want to renew or refinish your system – see below.

Renewing and Refinishing Seamless Flooring and Seamless Floor Coating Systems

Epoxy.com Epoxy and Urethane Seamless Flooring and Seamless Floor Coating Systems are designed to withstand heavy traffic and wear.  However, if there is enough traffic and/or abuse to cause the system to loose its shine, or show visible signs of wear, you may wish to restore the floor by “re-glazing” it.  Before re-glazing a flooring system or coating system you need to do the following:

  • Remove all wax, oil, grease and other contaminants from the surface
  • Lightly sand to break the shine
  • Consult with Epoxy.com Technical Support Department for the proper material to re-glaze you floor.  Be sure to follow all directions for installing the re-glazing material.

When in doubt contact Epoxy.com Technical Support at: info@epoxy.com or call us at 352-533-2167. You can also visit our website 24 hours per day at www.epoxy.com


Chemical Resistant Epoxy Selection

October 20, 2016

Requirements for a Chemical Resistant Epoxy or Vinyl Ester


Our Epoxy and Vinyl Ester product lines has extensive uses in Chemical Containment
and Chemical Resistance projects. The kind of product and systems we recommend are
based on a number of factors.  First we need to know exactly what you are doing:

  1. Are you patching concrete that has been damaged already? If so what is the extent
    of the damage?
  2. Do you need a secondary containment coating? If so what kind of traffic (if any)
    will this area see? Many of our systems will handle very heavy traffic.
  3. Are there any cracks that need repairing? If so how many lineal feet of cracks
    are there, what is the average depth and what is the average width. Repairing the cracks
    is the first step in making your project water and chemical tight.
  4. Are you looking to grout tile? We have chemically resistant Epoxy Tile Grout that
    has excellent chemical resistance.
  5. Is there any petroleum oil saturated concrete in the area. If so we have a product
    for that too.
  6. Is there any moisture vapor that is being transmitted through the floor?  We
    have solutions for that so please bring that to our attention when you contact us.
  7. Is this in an area where Static Disruptive or Conductive materials are needed (typically
    only in an explosive environment or where delicate electronics must be protected
    from static discharge).
  8. Total square footage of area requiring Chemical
    Resistant Epoxy or Vinyl Ester.

Then we will need to know some specifics about the chemical you are trying to protect
against:

  1. What is the specific chemical (or chemicals) that you are trying to resist against?
  2. What is the specific concentration of the chemical (or chemicals)?
  3. What is the duration of the exposure, before it will be cleaned up (if ever)?
  4. Is the exposure at an elevated temperature? If so what is that temperature, and
    how long will the chemicals be at this elevated temperature

If you have this information when you contact us, we can quickly help you to decide
what chemical resistant system is best and most economical for you.

Here is some additional reading that might interest you.

logo

For more information contact Epoxy.com Technical Support at info@epoxy.com or by calling us at 352-533-2167.


New Conductive Epoxy Primer

September 15, 2016

Epoxy.com is proud to announce Product #659. This is a  conductive primer that makes our existing conductive epoxy topcoat products even better.  Here is summary of the material:


CONDUCTIVE EPOXY PRIMER

Epoxy.com Product #659


DESCRIPTION

Product #659 Conductive Epoxy Primer is a water-based, two component, carbon filled conductive epoxy primer designed for use with various Epoxy.com Conductive Systems.Product #659  has very low odor making it suitable for use in occupied buildings.

ADVANTAGES

  • For Use with Various Epoxy.com Conductive Systems
  • Maintains Electrical Conductivity Performance over the Wear Life of the System
  • Fast Dry Time
  • Low Odor During Application and Cure
  • VOC Compliant in all 50 US States, Meets USGBC LEED Requirements

CONSIDERATIONS

  • Substrate must be above 50°F and relative humidity below 85% for proper curing.
  • Substrate must be properly prepared following Epoxy.com recommendations and free of dirt, waxes, curing agents and other foreign materials
  • Excessive moisture in the substrate will require a moisture vapor control treatment like Product #830
  • Concrete substrate must be insulated with a non-conductive
    epoxy primer/base coat like Product #12 Chemical Resistant Epoxy Primer or Product #899 Epoxy Primer  prior to application of Product #659 Conductive Epoxy Primer. Consult with Epoxy.com Technical Department for recommendations.
  • Must be top coated with a conductive top coating like Product #1ESD, or Product #630 Conductive.

APPLICATION

SURFACE PREPARATION

Surface Preparation is the most critical portion of any successful resinous flooring system application. All substrates must be properly prepared and tested for moisture as outlined in installation procedures or as recommended by Epoxy.com.

BATCHING, MIXING & INSTALLATION

 

Product #659 Conductive Epoxy Primer:
PART A 1 quart to
PART B 3 quarts to
Clean Water 8 volume ounces (6% by volume of water)
Total 4.125 quarts

Coverage (250 square feet/gal.) 265.6 square feet per batch

Pre-mix Product #659 Conductive Epoxy Primer  part B prior to combining with part A. Mix 1 part A with 3 parts B for 2-3 minutes with a low-speed jiffy mixer, scraping sides and bottom of mix vessel. Continue mixing and add 6% by volume clean potable water and continue mixing for 1 additional minute.

Immediately spread and back roll mixed Product #659 Conductive Epoxy Primer at a rate of 250 ft2 per gallon with a short nap roller over previously applied non-conductive epoxy primer/base coat.Care should be taken to avoid puddles. Allow to cure minimum 12 hours (at 75°F) to maximum 24 hours before coating with specified topcoat.

Important: Test Product #659 Conductive Epoxy Primer with ohm meter prior to top coating to confirm acceptable level of conductivity is achieved. If test readings are higher than 25,000 ohms, contact Epoxy.com Technical Support Department for further instructions before installing specified topcoat.

Top Coat with a conductive top coating like Product #1ESD, or Product #630 Conductive.

CLEAN-UP

Clean skin with soap and water. Tools and equipment should be cleaned with warm soapy water, xylene or lacquer thinner. Consult Material Safety Data for safety and health precautions.

COMPOSITION

Waterborne Epoxy Resin and Conductive Filler. Color: Black.

COVERAGE

Product #659 Conductive Epoxy Primer applied at 250 ft2 per gallon yields 2.7 mils dry film thickness.

TECHNICAL DATA (@ 75°F, 50% RH)

Viscosity 500-1000 CPS
Mixing Ratio 1 Part A to 3 Parts B by Volume
Solids Content, by volume 45%, thinned
Volatile Organic Content (VOC) <10 g/L
Bond Strength to Concrete 300-400+ psi (100% concrete failure)
Shelf Life 6 months when properly stored

CURE/DRY TIME (@ 75°F, 50% RH)

Pot Life 20-30 minutes
Dry to Touch 6-8 hours
Recoat (Refer to testing requirements) 12-24 hours
 Light Traffic 24 hours

For more information, visit us on line at Epoxy.com, email me at norm@epoxy.com or call Epoxy.com Technical Support at 352-533-2167.

Please join us on Facebook and Twitter.


Patching Vinyl Ester Floors With Novolac

July 28, 2016

A customer writes:

“We have a dairy processing and packaging facility that was built circa 1994.  At the time of construction we chose to install a flooring system which was vinyl ester based with fiberglass mat.  The floor has held up quite well in areas where it had a good bond.  The failures we have seen are in areas that covered either an expansion joint or control joint in the concrete.  In these areas the flooring has delaminated from the concrete.  Where possible we have made a clean cut through the flooring to an area where we had a good bond and left the concrete exposed.  Other failure areas are around floor drains.  We have made repairs with quick curing epoxies in the past but these don’t seem to bond well to the existing vinyl ester flooring. 

“Having a manufacturing facility with only one down day limits our ability to make substantive repairs.  During a search for low or no VOC  flooring systems I you folks.”

I have personally made many thousands of square feet of floor repairs that sounds exactly like the issues and conditions that you are describing.

Here is what I did to permanently resolve the issue, at least in the patched areas.

  1. Cut back the edges of the delaminated areas back to a point where the vinyl ester is well attached.
  2. Prep the concrete under the failed area and the edges of the old material – epoxy.com/surfaceprep.aspx.
  3. Prime with Epoxy.com Product #12 – epoxy.com/12.aspx
  4. Install a trowel coat of Epoxy.com Product #630 – epoxy.com/633.aspx and
    1. Epoxy Mortar Blend aggregate #82 Mortar Blend Aggregate
    2. Allow to cure hard to the touch and cool.
  5. Glaze with a neat coat of Epoxy.com Product #633 with optional Anti-skid – http://epoxy.com/non-skid-additive-polycarbonate-aggregate.aspx

Please email your additional questions to norm@epoxy.com or visit http://www.epoxy.com .